5.9.2011 ob 14:39
..torej gre za vrtno pot, lokacija primorska obala, iz Semmelrock plosc 60x30cm, barva anthrazit
model Caratstruktur, z zascito Preimum protect.
<!-- m --><a class="postlink" href="http://www.semmelrock.com/produkte/platten/detail.html?id=/_data/products/products/carat-struktur-platte.html">http://www.semmelrock.com/produkte/plat ... latte.html</a><!-- m -->
glede na visje temerature na obali se priporoca (Semmelrockov strokovnjak) fuge sirine od 8-10mm, delati pri zunanjih temeraturah od 15-20 stopinj, oblacno vreme(torej ne na soncu)
Priporocljiva fugirna masa: serije Sopro TNF, anthrazit
<!-- m --><a class="postlink" href="http://www.sopro.com/products/tfp/fliesentechnik/fgm/fugenmassen/46512/tnf.html">http://www.sopro.com/products/tfp/flies ... 2/tnf.html</a><!-- m -->
plosce bodo lepljene na trdo, betonsko podlago 10cm z lepilom Sopro MDM 888:
<!-- m --><a class="postlink" href="http://www.sopro.com/products/tfp/fliesentechnik/fnk/fliesen-natursteinkleber/46600/mdm_888.html">http://www.sopro.com/products/tfp/flies ... m_888.html</a><!-- m -->
zanima me kako fugirati med ploscami (debelina plosc 38mm)
1. kot ploscice, nanos fugirne mase na povrsino in potem brisanje le te z gobico
2. brizganje fugirne mase v rezo s "pistolo", ploscice zascititi ob fugi z lepilnim/zascitnim trakom, naenkrat pripraviti le 1-2kg fugirne mase...
Zadeva se zatakne, ko poslusas kako bi kdo delal:
-Avstrijc (Semmelrock strokovnjak, bil vodja gradbisc 20 let) pravi obvezno "2"
- slovenski keramicar pravi "1"
- hrvaski keramicar pravi "1"("2"- niko vam nece to praviti, to je je....e u ziv mozak)
kaken je torej pravilni postopek, saj plosc naj nebi "mazali" s fugirno maso vsepovprek...
hvala za odgovor
model Caratstruktur, z zascito Preimum protect.
<!-- m --><a class="postlink" href="http://www.semmelrock.com/produkte/platten/detail.html?id=/_data/products/products/carat-struktur-platte.html">http://www.semmelrock.com/produkte/plat ... latte.html</a><!-- m -->
glede na visje temerature na obali se priporoca (Semmelrockov strokovnjak) fuge sirine od 8-10mm, delati pri zunanjih temeraturah od 15-20 stopinj, oblacno vreme(torej ne na soncu)
Priporocljiva fugirna masa: serije Sopro TNF, anthrazit
<!-- m --><a class="postlink" href="http://www.sopro.com/products/tfp/fliesentechnik/fgm/fugenmassen/46512/tnf.html">http://www.sopro.com/products/tfp/flies ... 2/tnf.html</a><!-- m -->
plosce bodo lepljene na trdo, betonsko podlago 10cm z lepilom Sopro MDM 888:
<!-- m --><a class="postlink" href="http://www.sopro.com/products/tfp/fliesentechnik/fnk/fliesen-natursteinkleber/46600/mdm_888.html">http://www.sopro.com/products/tfp/flies ... m_888.html</a><!-- m -->
zanima me kako fugirati med ploscami (debelina plosc 38mm)
1. kot ploscice, nanos fugirne mase na povrsino in potem brisanje le te z gobico
2. brizganje fugirne mase v rezo s "pistolo", ploscice zascititi ob fugi z lepilnim/zascitnim trakom, naenkrat pripraviti le 1-2kg fugirne mase...
Zadeva se zatakne, ko poslusas kako bi kdo delal:
-Avstrijc (Semmelrock strokovnjak, bil vodja gradbisc 20 let) pravi obvezno "2"
- slovenski keramicar pravi "1"
- hrvaski keramicar pravi "1"("2"- niko vam nece to praviti, to je je....e u ziv mozak)
kaken je torej pravilni postopek, saj plosc naj nebi "mazali" s fugirno maso vsepovprek...